Journal of Metals, Materials and Minerals

Publication Date

2021

Abstract

In this present study, the development of a two-part geopolymer from waste red mud (RM) and silica fume (SF) by alkali activator is examined. The influence of silica fume addition, alkali concentration, curing duration are studied. The compressive strength of geopolymers has been achieved 0.8 MPa to 8 MPa with varying different compositions and synthesis parameters. The optimum RM/SF ratio is 60/40, the optimum solid/solution ratio is 1.8 gmL-1 or 2 gmL-1, and the optimum Na2SiO3/NaOH ratio is 0.5 day for 28 days curing time. The incorporation of iron in the geopolymer matrix contributes to geopolymerization. The study suggests that the produced geopolymer can be used as cementitious materials for making pavement and other valuable constructional materials. This procedure will be environment friendly and cheaper also.

DOI

10.55713/jmmm.v31i2.1004

First Page

10

Last Page

18

Share

COinS
 
 

To view the content in your browser, please download Adobe Reader or, alternately,
you may Download the file to your hard drive.

NOTE: The latest versions of Adobe Reader do not support viewing PDF files within Firefox on Mac OS and if you are using a modern (Intel) Mac, there is no official plugin for viewing PDF files within the browser window.