Journal of Metals, Materials and Minerals

Publication Date

2022

Abstract

Feedstock for powder injection moulding of silver was prepared using water-soluble binder composed of polyethylene glycol (PEG) and polyvinyl butyrol (PVB). Silver powders with particle size in range of 1 μm to 20 μm can be mixed with PEG/PVB binder system to form feedstocks having powder loadings of 42 vol% and 45 vol%. PEG can be removed using water leaching method while PVB can be removed by thermal debinding. Specimens retained their shapes during debinding and after debinding. Components fabricated with relatively higher powder loading resulted in higher density with lower porosity. Density of specimens containing powder loading of 42 vol% and 45 vol% and heated at 700℃ is about 43% and 46% of the theoretical value, respectively. Therefore, it can be further developed for porous materials applications.

DOI

10.55713/jmmm.v32i3.1271

First Page

75

Last Page

79

Share

COinS
 
 

To view the content in your browser, please download Adobe Reader or, alternately,
you may Download the file to your hard drive.

NOTE: The latest versions of Adobe Reader do not support viewing PDF files within Firefox on Mac OS and if you are using a modern (Intel) Mac, there is no official plugin for viewing PDF files within the browser window.